Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 4000A AR 15 TFE 15 SI 2  Polyphthalamide - Hot Water Mold (PPA) Aramid Fiber 15% - PTFE 15% - Silicone 2%

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Aramid Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4000A AR 15 TFE 15 SI 2  Polyphthalamide - Hot Water Mold (PPA) Aramid Fiber 15% - PTFE 15% - Silicone 2%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid Fiber 15% - PTFE 15% - Silicone 2%Comments:Aramid FiberPTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
0.0060 cm/cm

@Thickness 6.35 mm
0.0060 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Modulus of Elasticity 5.86 GPa
850 ksi
ASTM D638
Flexural Yield Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 316 - 338 °C
600 - 640 °F
Mold Temperature 65.6 - 163 °C
150 - 325 °F
Injection Pressure 68.9 - 103 MPa