Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 399 X 134920 A Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - Halogen Free

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 399 X 134920 A Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Preliminary Data Sheet
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0070 in/in

@Thickness 0.125 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D 638
Elongation at Break 5.0 - 10 %
5.0 - 10 %
ASTM D 638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D 638
Flexural Strength 82.7 MPa
12000 psi
ASTM D 790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D 790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity <= 10 ohm-cm
<= 10 ohm-cm
ASTM D 257
Surface Resistance <= 10000 ohm
<= 10000 ohm
ESD STM11.11
Surface Resistivity per Square <= 1e+05
<= 1e+05
ASTM D 257
Static Decay <= 0.50 sec
<= 0.50 sec
FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 271 - 299 °C
520 - 570 °F
Mold Temperature 65.6 - 104 °C
150 - 220 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content 0.020 %
0.020 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved