Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.8 MPa
9400 psi
ASTM D 638
Elongation at Break 10 %
10 %
ASTM D 638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D 638
Flexural Strength 107 MPa
15500 psi
ASTM D 790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D 790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D4812
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D 257
Surface Resistivity per Square 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 288 - 316 °C
550 - 600 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Drying Temperature 121 °C
250 °F
Dry Time 4 hour
4 hour
Moisture Content 0.020 %
0.020 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi