Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 399 X 115062 F Polycarbonate (PC), Carbon Nanotube - Electrically Conductive - ESD Protection - High Purity

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Conductive
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 399 X 115062 F Polycarbonate (PC), Carbon Nanotube - Electrically Conductive - ESD Protection - High Purity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.5 MPa
9500 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D 638
Flexural Strength 103 MPa
15000 psi
ASTM D 790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D 790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.20 mm
2.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Electrical Properties Metric English Comments
Volume Resistivity 10 - 1000 ohm-cm
10 - 1000 ohm-cm
ASTM D 257
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm
ESD STM11.11
Surface Resistivity per Square 10000 ohm - 1e+05
10000 ohm - 1e+05
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 288 - 316 °C
550 - 600 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content 0.020 %
0.020 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved