Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 3400 G-640  Liquid Crystal Polymer (LCP) Glass Fiber 40%  (discontinued **)&

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 3400 G-640  Liquid Crystal Polymer (LCP) Glass Fiber 40%  (discontinued **)&.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 40%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.00020 cm/cm

@Thickness 3.17 mm
0.00020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Modulus of Elasticity 24.1 GPa
3500 ksi
ASTM D638
Flexural Yield Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 17.9 GPa
2600 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
466 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 335 - 354 °C
635 - 670 °F
Mold Temperature 65.6 - 121 °C
150 - 250 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi