Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 3204  Ethylene Tetrafluoroethylene (ETFE) Glass Fiber 25%  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 3204  Ethylene Tetrafluoroethylene (ETFE) Glass Fiber 25%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 25%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.87 g/cc
1.87 g/cc
ASTM D792
Filler Content 25 %
25 %
Water Absorption 0.010 %
0.010 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
0.0030 cm/cm

@Thickness 6.35 mm
0.0030 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Modulus of Elasticity 5.86 GPa
850 ksi
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 13.9 J/cm

@Thickness 3.17 mm
26.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 274 - 335 °C
525 - 635 °F
Mold Temperature 65.6 - 149 °C
150 - 300 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black