  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 2.04 g/cc
2.04 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D 638
Elongation at Break 2.0 %
2.0 %
ASTM D 638
Tensile Modulus 6.21 GPa
900 ksi
ASTM D 638
Flexural Strength 55.2 MPa
8000 psi
ASTM D 790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D 790
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Processing Properties Metric English Comments
Melt Temperature 343 - 385 °C
650 - 725 °F
Mold Temperature 149 - 232 °C
300 - 450 °F
Drying Temperature 121 °C
250 °F
Dry Time 2 hour
2 hour
Injection Pressure 55.2 - 82.7 MPa
8000 - 12000 psi
Copyright © lookpolymers.com All Rights Reserved