Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 3183  Perfluoroalkoxy (PFA) Carbon Fiber 20%  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PFA , Fluorocarbon PFA with Carbon Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 3183  Perfluoroalkoxy (PFA) Carbon Fiber 20%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber 20%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 2.07 g/cc
2.07 g/cc
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.040 %
0.040 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
0.020 cm/cm

@Thickness 6.35 mm
0.020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Yield Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 86.4 µm/m-°C

@Temperature 20.0 °C
48.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.548 W/m-K
3.80 BTU-in/hr-ft²-°F
Through-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
400 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity >= 10.0 ohm-cm
>= 10.0 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 316 - 366 °C
600 - 690 °F
Mold Temperature 149 - 232 °C
300 - 450 °F
Injection Pressure 55.2 - 82.7 MPa
8000 - 12000 psi
Descriptive Properties Value Comments
Color Natural/Black