Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm @Thickness 3.17 mm |
0.013 - 0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 50 | 50 | instantaneous; ASTM D 2240 |
Tensile Strength at Break | 15.9 MPa | 2300 psi | ASTM D 638 |
Elongation at Break | 400 - 500 % | 400 - 500 % | ASTM D 638 |
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D 790 |
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
D 256 |
Izod Impact, Unnotched | NB @Thickness 3.17 mm |
NB @Thickness 0.125 in |
ASTM D4812 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flammability, UL94 | V-0 @Thickness 1.59 mm |
V-0 @Thickness 0.0625 in |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 210 °C | 360 - 410 °F | |
Mold Temperature | 15.6 - 65.6 °C | 60.0 - 150 °F | |
Drying Temperature | 79.4 °C | 175 °F | |
Dry Time | 2 hour | 2 hour | |
Moisture Content | 0.030 % | 0.030 % | |
Dew Point | -17.8 °C | 0.000 °F | |
Injection Pressure | 68.9 - 124 MPa | 10000 - 18000 psi |