Category | Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE |
Manufacturer | |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | RTP Company RTP 2740S-80A Unsaturated Styrenic Elastomer (SEBS) 80 Shore A - SEBS
(discont.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
Water Absorption | 0.050 % | 0.050 % | 24 hours at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 80 | 80 | ASTM D2240 |
Tensile Strength, Ultimate | 7.79 MPa | 1130 psi | ASTM D412 |
Elongation at Break | >= 480 % | >= 480 % | ASTM D412 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 171 - 199 °C | 340 - 390 °F | |
Mold Temperature | 15.6 - 37.8 °C | 60.0 - 100 °F | |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Natural/Black |