Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2740 S-45A Saturated Styrenic Block Copolymer (TES/SEBS or other)  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2740 S-45A Saturated Styrenic Block Copolymer (TES/SEBS or other)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0265 - 0.0347 cm/cm

@Thickness 3.17 mm
0.0265 - 0.0347 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
10 s delay; ASTM D 2240
Tensile Strength at Break 7.58 MPa
1100 psi
Break; Die C, 0.125 in (3.2mm)|^20 in/min (500 mm/min); ASTM D 412
Elongation at Break 1900 %
1900 %
Die C, 0.125 in (3.2mm)|^20 in/min (500 mm/min); ASTM D 412
Tear Strength 17.5 kN/m
100 pli
Die C; ASTM D 624
Processing Properties Metric English Comments
Melt Temperature 177 - 204 °C
350 - 400 °F
Mold Temperature 15.6 - 37.8 °C
60.0 - 100 °F
Drying Temperature 76.7 °C
170 °F
2 - 4 hrs
Moisture Content <= 0.040 %
<= 0.040 %
Injection Pressure 34.5 - 68.9 MPa
5000 - 10000 psi