Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2582 HEC FR Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant - UL94 V-0

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, NCG Fiber Filled , Polycarbonate (PC)
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2582 HEC FR Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber - EMI/RFI Shielding - Electrically Conductive - Flame Retardant - UL94 V-0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D 792
Additive Loading 15.0 %
15.0 %
Primary Additive
Linear Mold Shrinkage 0.000500 - 0.00250 cm/cm

@Thickness 3.20 mm
0.000500 - 0.00250 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 113 MPa
16400 psi
ASTM D 638
Elongation at Break 1.00 - 2.00 %
1.00 - 2.00 %
ASTM D 638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D 638
Flexural Strength 152 MPa
22000 psi
ASTM D 790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D 790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.20 mm
0.700 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.10 J/cm

@Thickness 3.20 mm
5.80 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity <= 10.0 ohm-cm
<= 10.0 ohm-cm
ASTM D 257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ESD STM11.11
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D 257; ESD STM11.11
Static Decay <= 0.500 sec
<= 0.500 sec
FTMS101C; 4046.1
Shielding Effectiveness 73.0 dB

@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
73.0 dB

@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
80.0 dB

@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
80.0 dB

@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
81.0 dB

@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
81.0 dB

@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
87.0 dB

@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
87.0 dB

@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
88.0 dB

@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
88.0 dB

@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
95.0 dB

@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
95.0 dB

@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
95.0 dB

@Thickness 2.00 mm,
Frequency 1.00e+9 Hz
95.0 dB

@Thickness 0.0787 in,
Frequency 1.00e+9 Hz
ASTM D 4935
100 dB

@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
100 dB

@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
100 dB

@Thickness 3.00 mm,
Frequency 1.00e+9 Hz
100 dB

@Thickness 0.118 in,
Frequency 1.00e+9 Hz
ASTM D 4935
101 dB

@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
101 dB

@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
102 dB

@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
102 dB

@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
105 dB

@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
105 dB

@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
Processing Properties Metric English Comments
Melt Temperature 243 - 274 °C
470 - 525 °F
Mold Temperature 51.7 - 93.3 °C
125 - 200 °F
Drying Temperature 93.3 °C

@Time 14400 sec
200 °F

@Time 4.00 hour
Moisture Content 0.0200 %
0.0200 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved