Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2303 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2303 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D 792
Filler Content 20 %
20 %
Primary Additive
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0015 - 0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
ASTM D 638
Elongation at Break 3.0 - 5.5 %
3.0 - 5.5 %
ASTM D 638
Tensile Modulus 5.52 GPa
800 ksi
ASTM D 638
Flexural Strength 172 MPa
25000 psi
ASTM D 790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D 790
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm
2.40 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 4.00 J/cm

@Thickness 3.17 mm
7.50 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 238 - 260 °C
460 - 500 °F
Mold Temperature 93.3 - 121 °C
200 - 250 °F
Drying Temperature 132 °C
270 °F
Dry Time 4 - 6 hour
4 - 6 hour
Moisture Content 0.010 %
0.010 %
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi