RTP Company RTP 2199 X 134911 A Polyetherimide (PEI) Nickel-Coated Carbon Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Nickel Coated Graphite Filled
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2199 X 134911 A Polyetherimide (PEI) Nickel-Coated Carbon Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D 792
Linear Mold Shrinkage 0.000500 cm/cm

@Thickness 3.20 mm
0.000500 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
24000 psi
ASTM D 638
Elongation at Break 1.00 - 2.00 %
1.00 - 2.00 %
ASTM D 638
Tensile Modulus 14.5 GPa
2100 ksi
ASTM D 638
Flexural Strength 207 MPa
30000 psi
ASTM D 790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D 790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.20 mm
1.30 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity <= 10.0 ohm-cm
<= 10.0 ohm-cm
ASTM D 257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ESD STM11.11
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D 257; ESD STM11.11
Static Decay <= 0.500 sec
<= 0.500 sec
FTMS101C; 4046.1
Shielding Effectiveness 65.0 dB

@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
65.0 dB

@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
68.0 dB

@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
68.0 dB

@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
73.0 dB

@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
73.0 dB

@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
77.0 dB

@Thickness 2.00 mm,
Frequency 1.00e+9 Hz
77.0 dB

@Thickness 0.0787 in,
Frequency 1.00e+9 Hz
ASTM D 4935
80.0 dB

@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
80.0 dB

@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
82.0 dB

@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
82.0 dB

@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
82.0 dB

@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
82.0 dB

@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
88.0 dB

@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
88.0 dB

@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
89.0 dB

@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
89.0 dB

@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
94.0 dB

@Thickness 3.00 mm,
Frequency 1.00e+9 Hz
94.0 dB

@Thickness 0.118 in,
Frequency 1.00e+9 Hz
ASTM D 4935
96.0 dB

@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
96.0 dB

@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
97.0 dB

@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
97.0 dB

@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
Processing Properties Metric English Comments
Melt Temperature 371 - 399 °C
700 - 750 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Drying Temperature 149 °C

@Time 14400 sec
300 °F

@Time 4.00 hour
Moisture Content 0.0400 %
0.0400 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi