Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2100 AR 15 TFE 10  Polyetherimide (PEI) Aramid Fiber 15% - PTFE 10%  (discon

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Aramid Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2100 AR 15 TFE 10  Polyetherimide (PEI) Aramid Fiber 15% - PTFE 10%  (discon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid Fiber 15% - PTFE 10%Comments:Aramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
0.0040 cm/cm

@Thickness 6.35 mm
0.0040 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Modulus of Elasticity 4.48 GPa
650 ksi
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.74 J/cm

@Thickness 3.17 mm
7.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
Through-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 349 - 382 °C
660 - 720 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black
Copyright © lookpolymers.com All Rights Reserved