Material Notes:
Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.25 %
0.25 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
0.0070 cm/cm

@Thickness 6.35 mm
0.0070 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
15000 psi
ASTM D638
Elongation at Break 7.5 %
7.5 %
ASTM D638
Modulus of Elasticity 2.96 GPa
430 ksi
ASTM D638
Flexural Yield Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 13.3 J/cm

@Thickness 3.17 mm
25.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Processing Properties Metric English Comments
Processing Temperature 349 - 382 °C
660 - 720 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black