Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2099 x 121825 E Biobased Polyamide (PA) Permanently Anti-static - ESD Protection - 31% Bio-Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2099 x 121825 E Biobased Polyamide (PA) Permanently Anti-static - ESD Protection - 31% Bio-Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D 792
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.20 mm
0.015 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 MPa
6000 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 1.72 GPa
250 ksi
ASTM D 638
Flexural Strength 55.2 MPa
8000 psi
ASTM D 790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D 790
Izod Impact, Notched 2.40 J/cm

@Thickness 3.20 mm
4.50 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 - 1.00e+10 ohm-cm
1.00e+9 - 1.00e+10 ohm-cm
ASTM D 257
Surface Resistivity per Square 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 218 - 246 °C
425 - 475 °F
Mold Temperature 51.7 - 79.4 °C
125 - 175 °F
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.00 hour
Moisture Content 0.20 %
0.20 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved