Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 208G HS L  Nylon 4/6 (PA 4/6) Glass Fiber 45% - Lubricated - Heat Stable  (d

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 208G HS L  Nylon 4/6 (PA 4/6) Glass Fiber 45% - Lubricated - Heat Stable  (d.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 45% - Lubricated - Heat StableComments:Glass FiberLubricatedHeat Stabilized(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Filler Content 45 %
45 %
Linear Mold Shrinkage 0.0035 cm/cm

@Thickness 3.17 mm
0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 224 MPa
32500 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Modulus of Elasticity 13.8 GPa
2000 ksi
ASTM D638
Flexural Yield Strength 347 MPa
50300 psi
ASTM D790
Flexural Modulus 13.4 GPa
1950 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm

@Thickness 3.17 mm
2.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm

@Thickness 3.17 mm
20.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
545 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 293 - 321 °C
560 - 610 °F
Mold Temperature 79.4 - 149 °C
175 - 300 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi