Category | Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler |
Manufacturer | |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | RTP Company RTP 205.3D HS Nylon 6/12 (PA 6/12) Glass Fiber 33% - Heat Stable
(discontinued.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Filler Content | 33 % | 33 % | |
Water Absorption | 0.25 % | 0.25 % | 24 hours at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 3.17 mm |
0.0040 in/in @Thickness 0.125 in |
ASTM D955 |
0.0050 cm/cm @Thickness 6.35 mm |
0.0050 in/in @Thickness 0.250 in |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 121 | 121 | ASTM D785 |
Tensile Strength, Ultimate | 152 MPa | 22000 psi | ASTM D638 |
Elongation at Break | 3.0 - 4.0 % | 3.0 - 4.0 % | ASTM D638 |
Modulus of Elasticity | 8.96 GPa | 1300 ksi | ASTM D638 |
Flexural Yield Strength | 228 MPa | 33000 psi | ASTM D790 |
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Izod Impact, Unnotched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 218 °C | 425 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | ASTM D648 |
Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
Per testing by RTP Company; ASTM D635 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | ASTM D257 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 252 - 279 °C | 485 - 535 °F | |
Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
Injection Pressure | 68.9 - 124 MPa | 10000 - 18000 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Natural/Black |