Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 203D FR  Nylon 6/12 (PA 6/12) Glass Fiber 20% - Flame Retardant  (discontinu

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 203D FR  Nylon 6/12 (PA 6/12) Glass Fiber 20% - Flame Retardant  (discontinu.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 20% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.25 %
0.25 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
0.0050 cm/cm

@Thickness 6.35 mm
0.0050 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Modulus of Elasticity 7.58 GPa
1100 ksi
ASTM D638
Flexural Yield Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 199 °C
390 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 191 °C
375 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 18.7 kV/mm
475 kV/in
S/T; ASTM D149
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
Dry; ASTM D150
Processing Properties Metric English Comments
Processing Temperature 252 - 279 °C
485 - 535 °F
Mold Temperature 60.0 - 93.3 °C
140 - 200 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black
Copyright © lookpolymers.com All Rights Reserved