Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 203 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized - UL94 V-0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D 792
Filler Content 20 %
20 %
Primary Additive
Water Absorption 1.4 %
1.4 %
24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D 785
Tensile Strength at Break 110 MPa
16000 psi
ASTM D 638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D 638
Tensile Modulus 8.96 GPa
1300 ksi
ASTM D 638
Flexural Strength 186 MPa
27000 psi
ASTM D 790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D 790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
400 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 243 - 279 °C
470 - 535 °F
Mold Temperature 54.4 - 93.3 °C
130 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 2 hour
2 hour
Moisture Content 0.20 %
0.20 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi