RTP Company RTP 201D L  Nylon 6/12 (PA 6/12) Glass Fiber 10% - Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 201D L  Nylon 6/12 (PA 6/12) Glass Fiber 10% - Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 10% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Filler Content 10 %
10 %
Water Absorption 0.23 %
0.23 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
0.0060 cm/cm

@Thickness 6.35 mm
0.0060 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Compressive Yield Strength 100 MPa
14500 psi
ASTM D695
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.8 µm/m-°C

@Temperature 20.0 °C
26.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.303 W/m-K
2.10 BTU-in/hr-ft²-°F
Through-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 207 °C
405 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
395 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 19.7 kV/mm
500 kV/in
S/T; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
Dry; ASTM D150
Arc Resistance 115 sec
115 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 252 - 279 °C
485 - 535 °F
Mold Temperature 60.0 - 93.3 °C
140 - 200 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black