Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 69.6 MPa
10100 psi
ASTM D 638
Elongation at Break 60 %
60 %
ASTM D 638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D 638
Flexural Strength 97.2 MPa
14100 psi
ASTM D 790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D 790
Izod Impact, Notched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D 648
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 360 - 391 °C
680 - 735 °F
Mold Temperature 138 - 163 °C
280 - 325 °F
Drying Temperature 135 - 149 °C
275 - 300 °F
Dry Time 4 - 6 hour
4 - 6 hour
Moisture Content 0.050 %
0.050 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi