Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 200 B Nylon 6/10 (PA), Unfilled

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 200 B Nylon 6/10 (PA), Unfilled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D 792
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.17 mm
0.015 - 0.022 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D 638
Elongation at Break 90 %
90 %
ASTM D 638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D 638
Flexural Strength 86.2 MPa
12500 psi
ASTM D 790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D 790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 277 - 299 °C
530 - 570 °F
Mold Temperature 65.6 - 107 °C
150 - 225 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 hour
2 hour
Moisture Content 0.20 %
0.20 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi