Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 199 X 130883 B Polypropylene (PP), Glass Fiber - Cellulose Fiber - Chemically Coupled - Heat Stabilized - 30% Renewable Resource Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Wood Filled
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 199 X 130883 B Polypropylene (PP), Glass Fiber - Cellulose Fiber - Chemically Coupled - Heat Stabilized - 30% Renewable Resource Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D 638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
ASTM D 638
Tensile Modulus 4.48 GPa
650 ksi
ASTM D 638
Flexural Strength 103 MPa
15000 psi
ASTM D 790
Flexural Modulus 4.62 GPa
670 ksi
ASTM D 790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C
150 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
ASTM D 648
Processing Properties Metric English Comments
Melt Temperature 191 - 232 °C
375 - 450 °F
Mold Temperature 32.2 - 65.6 °C
90.0 - 150 °F
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi