Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1800A TFE 10  Polycarbonate/Acrylic Alloy (PC/PMMA)   (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic/Polycarbonate Alloy , Polycarbonate (PC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1800A TFE 10  Polycarbonate/Acrylic Alloy (PC/PMMA)   (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments:Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Modulus of Elasticity 2.21 GPa
320 ksi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 21.4 J/cm

@Thickness 3.17 mm
40.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
Processing Properties Metric English Comments
Processing Temperature 202 - 249 °C
395 - 480 °F
Mold Temperature 32.2 - 65.6 °C
90.0 - 150 °F
Injection Pressure 55.2 - 82.7 MPa
8000 - 12000 psi
Descriptive Properties Value Comments
Color Natural/Black
Copyright © lookpolymers.com All Rights Reserved