Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1503-55D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1503-55D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
Additive Loading 20 %
20 %
Primary Additive
Linear Mold Shrinkage 0.0017 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0017 - 0.0025 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
instantaneous; ASTM D 2240
Tensile Strength at Break 43.1 MPa
6250 psi
ASTM D 638
Elongation at Break 8.75 %
8.75 %
ASTM D 638
Tensile Modulus 2.28 GPa
330 ksi
ASTM D 638
Flexural Strength 50.0 MPa
7250 psi
ASTM D 790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D 790
Izod Impact, Notched 3.42 J/cm

@Thickness 3.20 mm
6.40 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 10.7 J/cm

@Thickness 3.20 mm
20.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
Mold Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Drying Temperature 100 °C

@Time 7200 - 10800 sec
212 °F

@Time 2.00 - 3.00 hour
Moisture Content <= 0.10 %
<= 0.10 %