Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
instantaneous; ASTM D 2240
Tensile Strength at Break 16.5 MPa
2400 psi
ASTM D 638
Elongation at Break 300 %
300 %
ASTM D 638
Tensile Modulus 0.345 GPa
50.0 ksi
ASTM D 638
Flexural Strength 11.0 MPa
1600 psi
ASTM D 790
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D 790
Izod Impact, Notched 4.54 J/cm

@Thickness 3.20 mm
8.50 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
Processing Properties Metric English Comments
Melt Temperature 210 - 238 °C
410 - 460 °F
Mold Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Drying Temperature 93.3 °C

@Time 7200 - 14400 sec
200 °F

@Time 2.00 - 4.00 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved