Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D 792
Filler Content 5 %
5 %
Primary Additive
Linear Mold Shrinkage 0.0043 - 0.0053 cm/cm

@Thickness 3.17 mm
0.0043 - 0.0053 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.1 MPa
2480 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 0.414 GPa
60.0 ksi
ASTM D 638
Flexural Strength 12.1 MPa
1760 psi
ASTM D 790
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D 790
Izod Impact, Notched 3.47 J/cm

@Thickness 3.17 mm
6.50 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 4.11 J/cm

@Thickness 3.17 mm
7.70 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Processing Properties Metric English Comments
Melt Temperature 210 - 238 °C
410 - 460 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Drying Temperature 104 °C
220 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi