RTP Company RTP 1500-82D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated - Preliminary Data

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1500-82D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated - Preliminary Data.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
Linear Mold Shrinkage 0.015 - 0.020 cm/cm

@Thickness 3.17 mm
0.015 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
instantaneous; ASTM D 2240
Tensile Strength at Break 32.8 MPa
4750 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Tensile Modulus 0.896 GPa
130 ksi
ASTM D 638
Flexural Modulus 0.896 GPa
130 ksi
ASTM D 790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D 648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 210 - 238 °C
410 - 460 °F
Mold Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Drying Temperature 93.3 °C
200 °F
Dry Time 2 - 4 hour
2 - 4 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi