Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
Manufacturer | RTP Company |
Trade Name | |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | RTP Company RTP 150 LF Polypropylene (PP), Low Flow - Unreinforced - Flame Retardant - UL94 V-0.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D 792 |
Water Absorption | 0.030 % | 0.030 % | 24 hrs @ 23°C; ASTM D 570 |
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm @Thickness 3.17 mm |
0.012 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Melt Flow | 0.50 - 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.50 - 1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 22.8 MPa | 3300 psi | ASTM D 638 |
Elongation at Break | >= 10 % | >= 10 % | ASTM D 638 |
Tensile Modulus | 1.65 GPa | 240 ksi | ASTM D 638 |
Flexural Strength | 37.9 MPa | 5500 psi | ASTM D 790 |
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D 790 |
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
D 256 |
Izod Impact, Unnotched | NB @Thickness 3.17 mm |
NB @Thickness 0.125 in |
ASTM D4812 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 113 °C | 235 °F | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 65.6 °C | 150 °F | ASTM D 648 |
Flammability, UL94 | V-0 @Thickness 1.59 mm |
V-0 @Thickness 0.0625 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D 257 |
Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
Dry; ASTM D 150 |
Dielectric Strength | 19.7 kV/mm | 500 kV/in | Short Term; in oil; ASTM D 149 |
Dissipation Factor | 0.0020 @Frequency 1.00e+6 Hz |
0.0020 @Frequency 1.00e+6 Hz |
Dry; ASTM D 150 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 32.2 - 65.6 °C | 90.0 - 150 °F | |
Melt Temperature | 191 - 232 °C | 375 - 450 °F | |
Drying Temperature | 79.4 °C | 175 °F | |
Dry Time | 2 hour | 2 hour |