Category | Polymer , Thermoplastic , Polyphenylsulfone (PPSU) |
Manufacturer | RTP Company |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | RTP Company RTP 1499 P X 125056 B Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D 792 |
Additive Loading | 15.0 % | 15.0 % | Primary Additive |
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 84.1 MPa | 12200 psi | ASTM D 638 |
Elongation at Break | 8.40 % | 8.40 % | ASTM D 638 |
Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D 638 |
Flexural Strength | 128 MPa | 18600 psi | ASTM D 790 |
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D 790 |
Izod Impact, Notched | 0.801 J/cm @Thickness 3.20 mm |
1.50 ft-lb/in @Thickness 0.126 in |
ASTM D 256 |
Izod Impact, Unnotched | NB @Thickness 3.20 mm |
NB @Thickness 0.126 in |
ASTM D 4812 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 10.0 ohm-cm | <= 10.0 ohm-cm | ASTM D 257 |
Surface Resistance | <= 10000 ohm | <= 10000 ohm | ESD STM11.11 |
Surface Resistivity per Square | <= 1e+05 | <= 1e+05 | ASTM D 257; ESD STM11.11 |
Static Decay | <= 0.500 sec | <= 0.500 sec | FTMS101C; 4046.1 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 343 - 377 °C | 650 - 710 °F | |
Mold Temperature | 135 - 177 °C | 275 - 350 °F | |
Drying Temperature | 149 °C @Time 21600 sec |
300 °F @Time 6.00 hour |
|
Moisture Content | 0.0400 % | 0.0400 % | |
Dew Point | -31.7 °C | -25.0 °F | |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi |