Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1482 AR 10  Polyethersulfone (PES) Carbon Fiber 15% - Aramid Fiber 10%  (dis

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone, Carbon Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1482 AR 10  Polyethersulfone (PES) Carbon Fiber 15% - Aramid Fiber 10%  (dis.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber 15% - Aramid Fiber 10%Comments:Carbon FiberAramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Filler Content 15 %
15 %
Water Absorption 0.40 %
0.40 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
0.0020 cm/cm

@Thickness 6.35 mm
0.0020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Modulus of Elasticity 13.8 GPa
2000 ksi
ASTM D638
Flexural Yield Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 207 °C
405 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments