RTP Company RTP 1405 B  Polyethersulfone (PES) Glass Fiber 30%  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 30%Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1405 B  Polyethersulfone (PES) Glass Fiber 30%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.59 g/cc
1.59 g/cc
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.35 %
0.35 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
0.0020 cm/cm

@Thickness 6.35 mm
0.0020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 148 MPa
21500 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Modulus of Elasticity 10.3 GPa
1500 ksi
ASTM D638
Flexural Yield Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.2

@Frequency 1e+6 Hz
4.2

@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 15.0 kV/mm
380 kV/in
S/T; ASTM D149
Dissipation Factor 0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
Dry; ASTM D150
Arc Resistance 75 sec
75 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black