Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1402 N Z  Polyethersulfone (PES) Glass Fiber 15% - FDA Type - High Viscosity &nbs

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 20%Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1402 N Z  Polyethersulfone (PES) Glass Fiber 15% - FDA Type - High Viscosity &nbs.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 15% - FDA Type - High ViscosityComments:Glass FiberFDA CompliantHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Filler Content 15 %
15 %
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ASTM D638
Modulus of Elasticity 4.83 GPa
700 ksi
ASTM D638
Flexural Yield Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black
Copyright © lookpolymers.com All Rights Reserved