RTP Company RTP 1402 L  Polyethersulfone (PES) Glass Fiber 15% - Lubricated  (discontinued *

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 20%Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1402 L  Polyethersulfone (PES) Glass Fiber 15% - Lubricated  (discontinued *.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 15% - LubricatedComments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Filler Content 15 %
15 %
Water Absorption 0.40 %
0.40 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
0.0040 cm/cm

@Thickness 6.35 mm
0.0040 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Modulus of Elasticity 5.86 GPa
850 ksi
ASTM D638
Flexural Yield Strength 176 MPa
25500 psi
ASTM D790
Flexural Modulus 4.96 GPa
720 ksi
ASTM D790
Compressive Yield Strength 124 MPa
18000 psi
ASTM D695
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C

@Temperature 20.0 °C
22.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.288 W/m-K
2.00 BTU-in/hr-ft²-°F
Through-plane; ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 14.8 kV/mm
375 kV/in
S/T; ASTM D149
Dissipation Factor 0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
Dry; ASTM D150
Arc Resistance 70 sec
70 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black