Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
Water Absorption 0.370 %

@Time 86400 sec
0.370 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage 0.00600 cm/cm

@Thickness 3.20 mm
0.00600 in/in

@Thickness 0.126 in
ASTM D 955
Melt Flow 14.0 - 22.0 g/10 min

@Load 5.00 kg,
Temperature 365 °C
14.0 - 22.0 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 69.6 MPa
10100 psi
ASTM D 638
Elongation at Break 90.0 %
90.0 %
ASTM D 638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D 638
Flexural Strength 91.0 MPa
13200 psi
ASTM D 790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D 790
Izod Impact, Notched 6.94 J/cm

@Thickness 3.20 mm
13.0 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 343 - 388 °C
650 - 730 °F
Mold Temperature 138 - 163 °C
280 - 325 °F
Drying Temperature 149 °C

@Time 21600 sec
300 °F

@Time 6.00 hour
Moisture Content 0.0400 %
0.0400 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 138 MPa
10000 - 20000 psi