Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1383 TFE 10  Polyphenylene Sulfide (PPS) Carbon Fiber 20% - PTFE 10%  (disco

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1383 TFE 10  Polyphenylene Sulfide (PPS) Carbon Fiber 20% - PTFE 10%  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber 20% - PTFE 10%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.020 %
0.020 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
0.0020 cm/cm

@Thickness 6.35 mm
0.0020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Modulus of Elasticity 17.9 GPa
2600 ksi
ASTM D638
Flexural Yield Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 17.2 GPa
2500 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 1000 ohm-cm
10.0 - 1000 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 288 - 321 °C
550 - 610 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments