RTP Company RTP 1382 AR 15  Polyphenylene Sulfide (PPS) Carbon Fiber 15% - Aramid Fiber 15%  

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1382 AR 15  Polyphenylene Sulfide (PPS) Carbon Fiber 15% - Aramid Fiber 15%  .pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber 15% - Aramid Fiber 15%Comments:Carbon FiberAramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Filler Content 15 %
15 %
Water Absorption 0.020 %
0.020 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.00050 cm/cm

@Thickness 3.17 mm
0.00050 in/in

@Thickness 0.125 in
ASTM D955
0.0010 cm/cm

@Thickness 6.35 mm
0.0010 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
ASTM D638
Elongation at Break 0.50 %
0.50 %
ASTM D638
Modulus of Elasticity 26.2 GPa
3800 ksi
ASTM D638
Flexural Yield Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 19.3 GPa
2800 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Processing Properties Metric English Comments
Processing Temperature 288 - 321 °C
550 - 610 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black