Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1300 C TFE 15 Polyphenylene Sulfide (PPS), PTFE Lubricated

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with PTFE Filler
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1300 C TFE 15 Polyphenylene Sulfide (PPS), PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D 792
Filler Content 15 %
15 %
Primary Additive
Linear Mold Shrinkage 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D 638
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ASTM D 638
Tensile Modulus 3.24 GPa
470 ksi
ASTM D 638
Flexural Strength 117 MPa
17000 psi
ASTM D 790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D 790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 302 - 343 °C
575 - 650 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Drying Temperature 121 °C
250 °F
Dry Time 4 hour
4 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved