Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1200 S-65D TFE 10 Ester-based Thermoplastic Polyurethane Elastomer, PTFE Lubricated

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1200 S-65D TFE 10 Ester-based Thermoplastic Polyurethane Elastomer, PTFE Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D 792
Filler Content 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
instantaneous; ASTM D 2240
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D 638
Elongation at Break >= 400 %
>= 400 %
ASTM D 638
Flexural Modulus 0.276 GPa
40.0 ksi
ASTM D 790
Processing Properties Metric English Comments
Melt Temperature 160 - 218 °C
320 - 425 °F
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
Drying Temperature 107 °C
225 °F
Dry Time 6 hour
6 hour
Moisture Content 0.010 %
0.010 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 68.9 - 103 MPa