RTP Company RTP 1200 S-55D UV Ester-based Thermoplastic Polyurethane Elastomer, UV Stabilized

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1200 S-55D UV Ester-based Thermoplastic Polyurethane Elastomer, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
instantaneous; ASTM D 2240
Tensile Strength at Break 49.0 MPa
7100 psi
ASTM D 412
Tensile Strength, Yield 15.3 MPa

@Strain 50.0 %
2220 psi

@Strain 50.0 %
ASTM D 412
16.2 MPa

@Strain 100 %
2350 psi

@Strain 100 %
ASTM D 412
35.9 MPa

@Strain 300 %
5200 psi

@Strain 300 %
ASTM D 412
Elongation at Break 420 %
420 %
ASTM D 412
Flexural Modulus 0.172 GPa
25.0 ksi
ASTM D 790
Tear Strength 175 kN/m
1000 pli
Die C; ASTM D 624
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
400 - 430 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Drying Temperature 107 °C
225 °F
Dry Time 6 hour
6 hour
Moisture Content 0.020 %
0.020 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 41.4 - 103 MPa
6000 - 15000 psi