Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company ESD C 780 High Density Polyethylene (HDPE), Carbon Fiber - ESD Protection - Electrically Conductive

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer RTP Company
Trade Name ESD
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company ESD C 780 High Density Polyethylene (HDPE), Carbon Fiber - ESD Protection - Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D 638
Elongation at Break 6.0 - 10 %
6.0 - 10 %
ASTM D 638
Tensile Modulus 5.52 GPa
800 ksi
ASTM D 638
Flexural Strength 41.4 MPa
6000 psi
ASTM D 790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D 790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ASTM D 257
Surface Resistance <= 1e+05
<= 1e+05
ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohm
<= 1.00e+6 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 193 - 232 °C
380 - 450 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 hour
2 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved