RTP Company ESD C 1780  Modified Polyphenylene Oxide (PPO) Conductive - Carbon Fiber  (disco

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , PPE/PPO + Carbon Fiber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company ESD C 1780  Modified Polyphenylene Oxide (PPO) Conductive - Carbon Fiber  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive - Carbon FiberComments:ConductiveESD ProtectionCarbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
0.0020 cm/cm

@Thickness 6.35 mm
0.0020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D638
Modulus of Elasticity 8.62 GPa
1250 ksi
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 1.87 J/cm

@Thickness 3.17 mm
3.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D635
Electrical Properties Metric English Comments
Electrical Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
ASTM D257
Surface Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
ASTM D257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS-4046.1
Processing Properties Metric English Comments
Processing Temperature 232 - 282 °C
450 - 540 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black