RTP Company ESD A 2100 Polyetherimide (PEI), ESD Protection

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer RTP Company
Trade Name ESD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company ESD A 2100 Polyetherimide (PEI), ESD Protection.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.4 MPa
10500 psi
ASTM D 638
Elongation at Break 2.0 %
2.0 %
ASTM D 638
Tensile Modulus 4.14 GPa
600 ksi
ASTM D 638
Flexural Strength 165 MPa
24000 psi
ASTM D 790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D 790
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Electrical Properties Metric English Comments
Volume Resistivity <= 9.90e+6 ohm-cm
<= 9.90e+6 ohm-cm
ASTM D 257
Surface Resistance <= 9.90e+7 ohm
<= 9.90e+7 ohm
ESD STM11.11
Surface Resistivity per Square <= 9.90e+8 ohm
<= 9.90e+8 ohm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 354 - 399 °C
670 - 750 °F
Drying Temperature 149 °C
300 °F
Dry Time 4 hour
4 hour
Moisture Content 0.040 %
0.040 %
Dew Point -28.9 °C
-20.0 °F