Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company ESD 3281 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Static Dissipative

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
Manufacturer RTP Company
Trade Name ESD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company ESD 3281 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Static Dissipative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.71 g/cc
1.71 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.2 MPa
5100 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D 638
Flexural Strength 56.5 MPa
8200 psi
ASTM D 790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D 790
Izod Impact, Notched 8.01 J/cm

@Thickness 3.20 mm
15.0 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 16.0 J/cm

@Thickness 3.20 mm
30.0 ft-lb/in

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ASTM D 257
Surface Resistance <= 1.00e+8 ohm
<= 1.00e+8 ohm
ESD STM11.11
Surface Resistivity per Square <= 1.00e+9 ohm
<= 1.00e+9 ohm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 293 - 343 °C
560 - 650 °F
Mold Temperature 65.6 - 149 °C
150 - 300 °F
Drying Temperature 121 °C

@Time 7200 sec
250 °F

@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved