Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company EMI 331 F FR Polycarbonate (PC), 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer RTP Company
Trade Name EMI
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company EMI 331 F FR Polycarbonate (PC), 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D 792
Filler Content 12.5 %
12.5 %
Primary Additive
Linear Mold Shrinkage 0.0025 - 0.0035 cm/cm

@Thickness 3.17 mm
0.0025 - 0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 89.6 MPa
13000 psi
ASTM D 638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D 638
Tensile Modulus 5.38 GPa
780 ksi
ASTM D 638
Flexural Strength 145 MPa
21000 psi
ASTM D 790
Flexural Modulus 5.38 GPa
780 ksi
ASTM D 790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity <= 1.0 ohm-cm
<= 1.0 ohm-cm
ASTM D 257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ESD STM11.11
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 277 - 304 °C
530 - 580 °F
Mold Temperature 71.1 - 121 °C
160 - 250 °F
Drying Temperature 121 °C
250 °F
Dry Time 4 hour
4 hour
Moisture Content 0.020 %
0.020 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved