Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company EMI 263 Nylon 6/6 (PA), Stainless Steel Fiber - EMI/RFI/ESD Protection

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Stainless Steel Filled; EMI Grade
Manufacturer RTP Company
Trade Name EMI
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company EMI 263 Nylon 6/6 (PA), Stainless Steel Fiber - EMI/RFI/ESD Protection.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D 792
Filler Content 20 %
20 %
Primary Additive
Linear Mold Shrinkage 0.010 - 0.014 cm/cm

@Thickness 3.17 mm
0.010 - 0.014 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
ASTM D 638
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
ASTM D 638
Tensile Modulus 4.83 GPa
700 ksi
ASTM D 638
Flexural Strength 124 MPa
18000 psi
ASTM D 790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D 790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Electrical Properties Metric English Comments
Volume Resistivity <= 1.0 ohm-cm
<= 1.0 ohm-cm
ASTM D 257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ESD STM11.11
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 252 - 293 °C
485 - 560 °F
Mold Temperature 79.4 - 98.9 °C
175 - 210 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 4 hour
4 hour
Moisture Content 0.20 %
0.20 %
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi