Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%  (disc

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Nickel Coated Graphite Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%  (disc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shielding - Nickel-Coated Carbon Fiber 20%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.20 %
0.20 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm

@Thickness 3.17 mm
0.0015 - 0.0025 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D638
Modulus of Elasticity 11.0 GPa
1600 ksi
ASTM D638
Flexural Yield Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.8 µm/m-°C

@Temperature 20.0 °C
6.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity <= 1.00 ohm-cm
<= 1.00 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS-4046.1
Processing Properties Metric English Comments
Processing Temperature 349 - 382 °C
660 - 720 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black