Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It offers fast molding cycles and good surface appearance. Form and Colors = Roll, Off White/Black/Gray. Glass Length = 1 inch.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 58
58
ASTM D2583
Tensile Strength, Ultimate 193 MPa
28000 psi
ASTM D638
Tensile Modulus 17.9 GPa
2600 ksi
ASTM D638
Flexural Yield Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 14.5 GPa
2100 ksi
ASTM D790
Compressive Yield Strength 172 MPa
24900 psi
ASTM D695
Izod Impact, Notched 14.4 J/cm
27.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Shrinkage 0.0010 %
0.0010 %
Processing Properties Metric English Comments
Processing Temperature 132 - 157 °C
270 - 315 °F
Mold temperature